In short
- Loss is created at loading, not in the kiln: crate height, pallet pattern and moisture decide which tiles survive the sea leg.
- A BIII body can take more than 20 times the water of a BIa body, so one wet crossing marks one load and saturates another.
- No published loss rate applies to your order. Count refused crates against shipped crates, with a survey taken before stripping.
Tile packing is the system of crates, pallets, interleaves and restraints that carries fired tiles from factory to site, and container loading is the plan that fits those units into a box within its mass and volume limits. The loss rate is the share of ordered area that arrives unusable, counted against a survey taken before the container is stripped.
Buyers ask for that percentage as though a standard one exists. It does not. Loss depends on the body, the crate drawing, the stack height, the season, the handlings and the port, and a figure borrowed from another buyer's container describes another buyer's container. What can be quoted is the arithmetic, and what can be specified is the packing.
01The loss rate is a ratio you calculate, not a figure you quote
Loss is unusable area divided by delivered area, counted when a crate is opened. A supplier who offers a percentage before seeing the crate drawing, the stack height and the route is describing their own experience, not your risk.
Loss is not one event. It accumulates at six points between the kiln and the fixed floor, and each leaves different evidence. A buyer who knows which point produced the damage knows who to claim against; one who opens a broken container usually knows neither.
| Stage | What fails | Evidence that survives | Usual bearer |
|---|---|---|---|
| Factory packing | Arris chips, thin interleave, tight banding | Crate opened, before the lid is fixed | Supplier |
| Loading | Overhang, uneven stack, unblocked last row | Loading sequence photographs | Supplier or loader |
| Sea leg | Condensation, cargo shift, settlement | Survey at discharge, before stripping | Carrier, if surveyed |
| Port and haul | Impact at the spreader, then vibration | Tally, equipment report, delivery note | Terminal or hauler |
| Site storage | Damp store, crates on edge | Site log and store photographs | Buyer |
The table maps evidence, not blame. A row with no evidence cannot be argued, whichever party was at fault.
The ratio that survives a claim is refused crates over shipped crates. Both numbers sit on the packing list, both can be counted in front of a surveyor, and neither depends on an estimate.
02Crate height sets the load the bottom course carries
A stack of crates puts the whole stack's mass through the frame of the bottom one. Three high means the bottom crate carries three crates' worth of load; five high means five, transmitted through its frame to the lowest course of tiles.
Frames are usually designed for dry timber. Plywood and carton board take up moisture on a long sea leg, lose stiffness, and the load path moves from the frame onto the tile arris. The signature is chipped corners concentrated in the bottom crate, with the upper crates intact.
Height also meets a hard limit at the door. The aperture is lower than the internal height, so the last crate is where a loading plan breaks. Ask for the aperture in millimetres, and the clearance above the top crate.
Crate height is a freight decision too. Taller crates use volume a dense cargo does not need; shorter crates add handlings. The compromise is the tallest crate that still fits the stack its frame was designed for.
Catalogue reference: tiles and porcelain in the catalogue — models, dimensions and finishes for the directions discussed above.
03The pallet pattern decides which corner survives
Corners fail first, and the pattern decides whether a corner has anywhere to move. A tile restrained hard on its face and free at its arris will chip; one that can slide a millimetre under banding usually arrives whole.
Rectified tiles are cut to a calibrated size after firing, which is what allows a joint of about 2–3 mm. The same cut leaves a square arris that shows every knock: a 1 mm chip is obvious at a 3 mm joint and invisible on a pressed edge at 6 mm. Non-rectified tiles need a wider joint to absorb size variation, and their softer edge hides a knock that a rectified arris shows.
Non-rectified tiles carry size variation and need a wider joint to absorb it. That tolerance helps at the joint and complicates the pattern: the footprint varies more from tile to tile, so banding tension that suits one over-compresses the next.
| Pattern | What it protects | What it costs | Where it fails |
|---|---|---|---|
| Face to face with foam interleave | Decorated face and arris | Two interleaves per pair; extra height | Banding tension crushes the outer arris |
| Back to back, face outward | Face against face contact | Less void, fewer handlings | Outer faces touch the crate wall |
| Vertical or A-frame | Face and edges on large format | Floor area, frames, lifting gear | Frames not restrained fore and aft |
| Pallet and shrink wrap only | Dust and surface water | Nothing structural | The whole unit, at the first lift |
Patterns are usually combined: a vertical A-frame inside a crate, or back-to-back pairs inside a face-to-face block. Ask which combination, and where the banding crosses the tile.
Shade is the other reason to group at the pallet. Shade variation is declared V1 to V4, a guide across batches rather than a guarantee. Pack by shade and calibre per pallet and load in floor order; mix V3 stock across the container and the loss is one the factory never sees.
Shade is the other reason to group at the pallet. Shade variation is declared V1 to V4, a guide across batches rather than a guarantee. Pack by shade and calibre per pallet, load in floor order, and a room can be finished from one group; mix V3 stock across the container and the loss is one the factory never sees.
04Absorption class decides what a wet crossing does
Water absorption is the number that turns weather into damage, and ISO 13006 and EN 14411 sort ceramic tiles by it. The class belongs on the data sheet, not the carton.
| Group | Absorption | Water held per kg | What a wet crossing can do | Evidence |
|---|---|---|---|---|
| BIa | 0.5% or less | Up to 5 g | Surface condensation; dries from the face | ASTM C373 value |
| BIb | 0.5–3% | 5–30 g | Damp interleave, tide marks at the arris | ASTM C373 value |
| BIIa | 3–6% | 30–60 g | Carton softens, stack settles | C373 and packing spec |
| BIIb | 6–10% | 60–100 g | Body stays damp for the voyage | C373, C1026 if exterior |
| BIII | More than 10% | Over 100 g | Saturation, efflorescence, frost damage | C373 and C1026 |
Water held is calculated from the band: 0.5% of 1 kg is 5 g, 10% of 1 kg is 100 g, per kilogram of fired body.
A BIII body can take more than 20 times the water of a BIa body, kilogram for kilogram. A crossing that leaves a BIa face with a dried tide mark can leave a BIII body wet enough that the interleave and carton stay damp for the rest of the voyage.
The mechanism is condensation, not rain. Air loaded warm and humid cools at sea, condenses on the roof and the top of the stack, runs down and wicks into the packing. Damage clusters at the top crates, and at the bottom, where water collects and load is highest.
Frost is where a wet crossing becomes a warranty argument. Low absorption is not frost-proofing: the test is ASTM C1026, and a claim without a report naming that body and thickness is a sentence in a brochure. Spalling usually appears after the first winter, long after the container was signed for.
Slip ratings answer a different question again. DIN 51130 runs R9 to R13, DIN 51097 uses A, B and C for barefoot wet areas, and ANSI A326.3 measures wet DCOF, with 0.42 the common reference for level interior floors. None of them describes a body that has taken up water in transit.
05Weight out beats cube out, so the floor plan sets the load
Tiles are dense cargo: a box reaches its permitted mass long before it is full. The limit is not the height of the box but the mass on the floor and the stack the crates were designed for.
The CTU Code, the IMO/ILO/UNECE code of practice for packing cargo transport units, covers how mass is distributed and secured on sea and land legs, and it addresses packers and receivers alike. It is non-mandatory, which is why it belongs in the purchase order.
A loading plan has three jobs: keep mass low and centred, block the last row so it cannot move under braking, and leave no unsecured space above the stack. Empty volume over a dense cargo is a gap in which the stack works loose.
Crates on the floor multiplied by crates high gives the crate count in the box. Cutting the stack by one course does not cost one crate; it costs a floor's worth.
06The claim file is built before the doors close
A claim is decided by evidence made at packing, loading and discharge. Anything produced later is opinion.
- Packing photographs with the crate open: interleave thickness, corner protection, banding positions.
- Loading photographs in sequence: stack pattern, blocking, clearance to the roof.
- Container and seal numbers recorded on the packing list and in the photographs.
- A survey at destination before stripping, with the surveyor named and the time recorded.
- A delivery note on which every exception is written at the gate, by crate number.
- The batch and calibre list by crate, so a replacement can be matched rather than counted.
The common failure is procedural. The box is stripped, damage is found, and a surveyor is called to a floor of loose tiles with no container left to inspect. Damage can be proved; its origin cannot, and a carrier or insurer declines on that basis.
Keep the batch and calibre list with the crate numbers. A replacement from a later batch will not match a V3 floor, so the claim is settled in area and matching stock, not only in money.
07The second loss appears at the fixing
Transit damage and installation loss arrive together and get counted as one. The first is claimable. The second is designed in before the tiles are made, and paid for twice: in material and in labour.
A chipped corner becomes a lippage problem. The usual acceptance for rectified porcelain is a 1 mm step at a joint, checked against a straightedge, and a floor laid with a 2–3 mm joint has nowhere to hide a chip on the arris.
Large-format tiles need a C2TE-class adhesive to EN 12004, coverage of at least 90–95%, and a substrate flat to about 3 mm over 2 m. Miss any of the three and the cost is a re-lay, not a tile.
Coverage is worth one calculation. On a 1,200 × 600 mm tile the face is 0.72 m², so the gap between 90% and 95% coverage is 0.05 × 0.72 = 0.036 m² of void behind each tile. That void is where a hollow spot starts, and where a corner cracks under a point load.
Separating the two losses is commercial rather than academic. A buyer who counts them together cannot tell whether packing or fixing failed, and the remedy differs: a crate drawing on one side, an adhesive class and a flatness tolerance on the other.
What your RFQ should state
- The crate drawing, with internal dimensions, timber specification, corner protection and gross mass per crate.
- The maximum stack height in crates and in millimetres, with clearance to the container roof and door aperture.
- Crates on the floor and crates per stack, so the total count can be checked against the packing list.
- The body class to ISO 13006 with its ASTM C373 value, and an ASTM C1026 report where the destination freezes.
- An ASTM C648 breaking strength report for the supplied thickness and finish, not for the series.
- Shade and calibre grouped per pallet, marked on each crate and listed by crate number.
- Packing and loading photographs with container and seal numbers, sent before the vessel departs.
- A survey at destination before stripping, and replacement terms for any crate refused there.
Where this guidance stops
- Loss rates vary with body, crate design, route, season and handling count. Nothing here predicts your rate; it gives you the method to measure it.
- A crate photograph cannot show banding tension, interleave thickness or the moisture content of the timber at loading.
- Absorption class describes a body under test. A saturated tile and a dry tile of the same class behave differently on site.
- Frost and slip resistance are properties of a tested product and, for a floor, of the whole build-up. Local code and the fixing system decide.
- Foshan Supply coordinates sourcing, inspection and consolidation. We do not pack, load, survey or issue test reports, and we do not insure cargo.
Questions buyers ask
What is a normal breakage rate for tiles in a container?
There is no defensible industry figure, and a number from another buyer's container describes their body, crate and route. Build your own from refused crates divided by shipped crates, with a survey taken before stripping. Two orders on the same lane give a baseline; one order gives an anecdote.
How many crates high can tiles be stacked in a container?
It depends on the crate frame, the gross mass and the stack the frame was designed for, not on internal height alone. At three high the bottom crate carries three crates' worth of load. Ask for stack height in millimetres and clearance to the roof, then check the plan against the door aperture.
Does a wet container damage tiles?
It can, and the body decides how much. A BIa body at 0.5% absorption or less takes up little water; a BIII body above 10% can take more than 20 times as much. Condensation that marks one load can saturate another. Damage shows as tide marks, damp interleaves, efflorescence and, at a freezing destination, spalling.
Can porcelain tiles be called frost-proof?
Only with an ASTM C1026 freeze–thaw report for that body and thickness. Low absorption, at 0.5% or less in group BIa, is a good sign but not proof, and a tile saturated in transit is not the dry sample that was tested. Ask for the report rather than the word.
Do rectified tiles chip more in transit?
They are more likely to show a chip. Rectification cuts a calibrated, square arris that allows a 2–3 mm joint, and that sharp edge makes a 1 mm knock visible where a pressed edge would hide it. The answer is corner protection and a pattern that does not load the arris.
Who pays for tiles broken in transit?
It depends on where risk passes in your terms of sale and on what the survey can show. A survey at discharge, before stripping, separates a loading fault from a sea-leg event. Without one, a carrier or insurer can decline for want of attribution. Loading photographs are the other half of the file.
Should I order a spare percentage for breakage?
Order against a counted rate, not a habit. If your last container refused two crates of forty, that is the figure to plan with, in the same units as the packing list. Keep spares from the same batch and calibre, because later stock of V3 material will not match a floor laid from this one.
Sources
- ISO 13006:2018 — Ceramic tiles: definitions, classification, characteristics and marking — International Organization for Standardization
- ANSI A326.3 — Test method for measuring dynamic coefficient of friction of hard surface flooring — Tile Council of North America
- ASTM C373 — Standard test methods for determination of water absorption and bulk specific gravity of ceramic tile — ASTM International
- ASTM C648 — Standard test method for breaking strength of ceramic tile — ASTM International
- IMO/ILO/UNECE Code of Practice for Packing of Cargo Transport Units (CTU Code) — International Maritime Organization
- ASTM C1026 — Standard test method for measuring the resistance of ceramic tile to freeze-thaw cycling — ASTM International
- EN 12004 — Adhesives for ceramic tiles: classification and requirements — European Committee for Standardization
Pages related to this guide
How this guide was checked
- Written from the public catalogue, the standards and regulator pages listed under Sources, and the process records described on the services page.
- Catalogue references and model details were checked on 2026-11-05; 7 primary sources are linked above.
- No supplier paid for placement. No price on this page is an offer; ranges are planning references and must be confirmed in a quotation.
How these guides are researched and reviewed · Corrections policy